Zero resistance of quenched Bi1.5Pb0.4Sb0.1Sr2Ca2Cu3Ox at 140 K
Khan, J. A. A. ; Butt, N. M. ; Mahmood, A. ; Shaheen, R. ; Bashir, G. ; Shahid, K. A.
Springer
Published 1992
Springer
Published 1992
ISSN: |
1573-4803
|
---|---|
Source: |
Springer Online Journal Archives 1860-2000
|
Topics: |
Mechanical Engineering, Materials Science, Production Engineering, Mining and Metallurgy, Traffic Engineering, Precision Mechanics
|
Notes: |
Abstract A glass-ceramic of nominal composition Bi1.5Pb0.4Sb0.1Sr2Ca2Cu3Ox was prepared by the melt-quenching method. The subsequent heat treatment of the sample at 860±5°C showedT c(zero) at 94 K. Exposure of the sample for 4 days in air improved itsT c(zero) to 140 K. In another similarly heat-treated sample, a two-step transition in the p-Tcurve at 140 K and at 1 1 1 K, was observed. The superconducting transition appeared to be of a percolative nature.
|
Type of Medium: |
Electronic Resource
|
URL: |
_version_ | 1798296737250541569 |
---|---|
autor | Khan, J. A. A. Butt, N. M. Mahmood, A. Shaheen, R. Bashir, G. Shahid, K. A. |
autorsonst | Khan, J. A. A. Butt, N. M. Mahmood, A. Shaheen, R. Bashir, G. Shahid, K. A. |
book_url | http://dx.doi.org/10.1007/BF00576279 |
datenlieferant | nat_lic_papers |
hauptsatz | hsatz_simple |
identnr | NLM194636089 |
issn | 1573-4803 |
journal_name | Journal of materials science |
materialart | 1 |
notes | Abstract A glass-ceramic of nominal composition Bi1.5Pb0.4Sb0.1Sr2Ca2Cu3Ox was prepared by the melt-quenching method. The subsequent heat treatment of the sample at 860±5°C showedT c(zero) at 94 K. Exposure of the sample for 4 days in air improved itsT c(zero) to 140 K. In another similarly heat-treated sample, a two-step transition in the p-Tcurve at 140 K and at 1 1 1 K, was observed. The superconducting transition appeared to be of a percolative nature. |
package_name | Springer |
publikationsjahr_anzeige | 1992 |
publikationsjahr_facette | 1992 |
publikationsjahr_intervall | 8009:1990-1994 |
publikationsjahr_sort | 1992 |
publisher | Springer |
reference | 27 (1992), S. 6321-6323 |
search_space | articles |
shingle_author_1 | Khan, J. A. A. Butt, N. M. Mahmood, A. Shaheen, R. Bashir, G. Shahid, K. A. |
shingle_author_2 | Khan, J. A. A. Butt, N. M. Mahmood, A. Shaheen, R. Bashir, G. Shahid, K. A. |
shingle_author_3 | Khan, J. A. A. Butt, N. M. Mahmood, A. Shaheen, R. Bashir, G. Shahid, K. A. |
shingle_author_4 | Khan, J. A. A. Butt, N. M. Mahmood, A. Shaheen, R. Bashir, G. Shahid, K. A. |
shingle_catch_all_1 | Khan, J. A. A. Butt, N. M. Mahmood, A. Shaheen, R. Bashir, G. Shahid, K. A. Zero resistance of quenched Bi1.5Pb0.4Sb0.1Sr2Ca2Cu3Ox at 140 K Abstract A glass-ceramic of nominal composition Bi1.5Pb0.4Sb0.1Sr2Ca2Cu3Ox was prepared by the melt-quenching method. The subsequent heat treatment of the sample at 860±5°C showedT c(zero) at 94 K. Exposure of the sample for 4 days in air improved itsT c(zero) to 140 K. In another similarly heat-treated sample, a two-step transition in the p-Tcurve at 140 K and at 1 1 1 K, was observed. The superconducting transition appeared to be of a percolative nature. 1573-4803 15734803 Springer |
shingle_catch_all_2 | Khan, J. A. A. Butt, N. M. Mahmood, A. Shaheen, R. Bashir, G. Shahid, K. A. Zero resistance of quenched Bi1.5Pb0.4Sb0.1Sr2Ca2Cu3Ox at 140 K Abstract A glass-ceramic of nominal composition Bi1.5Pb0.4Sb0.1Sr2Ca2Cu3Ox was prepared by the melt-quenching method. The subsequent heat treatment of the sample at 860±5°C showedT c(zero) at 94 K. Exposure of the sample for 4 days in air improved itsT c(zero) to 140 K. In another similarly heat-treated sample, a two-step transition in the p-Tcurve at 140 K and at 1 1 1 K, was observed. The superconducting transition appeared to be of a percolative nature. 1573-4803 15734803 Springer |
shingle_catch_all_3 | Khan, J. A. A. Butt, N. M. Mahmood, A. Shaheen, R. Bashir, G. Shahid, K. A. Zero resistance of quenched Bi1.5Pb0.4Sb0.1Sr2Ca2Cu3Ox at 140 K Abstract A glass-ceramic of nominal composition Bi1.5Pb0.4Sb0.1Sr2Ca2Cu3Ox was prepared by the melt-quenching method. The subsequent heat treatment of the sample at 860±5°C showedT c(zero) at 94 K. Exposure of the sample for 4 days in air improved itsT c(zero) to 140 K. In another similarly heat-treated sample, a two-step transition in the p-Tcurve at 140 K and at 1 1 1 K, was observed. The superconducting transition appeared to be of a percolative nature. 1573-4803 15734803 Springer |
shingle_catch_all_4 | Khan, J. A. A. Butt, N. M. Mahmood, A. Shaheen, R. Bashir, G. Shahid, K. A. Zero resistance of quenched Bi1.5Pb0.4Sb0.1Sr2Ca2Cu3Ox at 140 K Abstract A glass-ceramic of nominal composition Bi1.5Pb0.4Sb0.1Sr2Ca2Cu3Ox was prepared by the melt-quenching method. The subsequent heat treatment of the sample at 860±5°C showedT c(zero) at 94 K. Exposure of the sample for 4 days in air improved itsT c(zero) to 140 K. In another similarly heat-treated sample, a two-step transition in the p-Tcurve at 140 K and at 1 1 1 K, was observed. The superconducting transition appeared to be of a percolative nature. 1573-4803 15734803 Springer |
shingle_title_1 | Zero resistance of quenched Bi1.5Pb0.4Sb0.1Sr2Ca2Cu3Ox at 140 K |
shingle_title_2 | Zero resistance of quenched Bi1.5Pb0.4Sb0.1Sr2Ca2Cu3Ox at 140 K |
shingle_title_3 | Zero resistance of quenched Bi1.5Pb0.4Sb0.1Sr2Ca2Cu3Ox at 140 K |
shingle_title_4 | Zero resistance of quenched Bi1.5Pb0.4Sb0.1Sr2Ca2Cu3Ox at 140 K |
sigel_instance_filter | dkfz geomar wilbert ipn albert fhp |
source_archive | Springer Online Journal Archives 1860-2000 |
timestamp | 2024-05-06T09:56:51.117Z |
titel | Zero resistance of quenched Bi1.5Pb0.4Sb0.1Sr2Ca2Cu3Ox at 140 K |
titel_suche | Zero resistance of quenched Bi1.5Pb0.4Sb0.1Sr2Ca2Cu3Ox at 140 K |
topic | ZL |
uid | nat_lic_papers_NLM194636089 |